Property | Test Method | Units | Value |
---|---|---|---|
Density* Tensile modulus Yield stress Elogation at break Charpy impact strengh Scracth resistance |
ISO 1183 ISO 178:2003 ISO 527 ISO 527 ISO 179/1fn DIN 68861T4 |
g/cm3 Mpa Mpa % KI/m2 N |
1,11 1800 38 35 23 0,6 |
HDT más. Long time application 23ºC temperature | ºC | 104 | |
Themoforming Temperature range |
ºC | 180 – 190 | |
Thermal estability Light fastness Top surface gloss |
UNE 13559 UNE 4892 |
Visual
1 – 8
GLE
|
OK
7
>85
|
Chemical agent resistance | UNE 5.4 | Visual | OK |
Burnin rate* nom 1,6 mm | ISO 1210 / UL94 | HB |
* Total colour difference after 200h Xenon test
** Flamability is rated on raw material data (>1,6mm.)